Cincin Seramik Alumina
Parameter Teknikal
Had Operasi | Unit | Seramik Alumina | Seramik Alumina |
Kandungan Alumina | wt% | ≥ 99 | ≥ 95 |
Ketumpatan Isipadu | g /cm3 | 3.85 | 3.7 |
Kekerasan (HRA) | HRA ≥ | 88 | 86 |
Kekuatan Mampatan | MPa ≥ | 400 | 300 |
Suhu Maksimum | ℃ | 1500 | 1500 |
Ujian Kedap Udara | lulus | lulus | |
Ujian Kejutan Terma | lulus | lulus | |
Pekali Pengembangan Haba | ×10-6/℃ | 8.2 | 7.5 |
Pemalar Dielektrik | εr20 ℃, 1MHz | 9.2 | 9 |
Kehilangan Dielektrik | tanδ×10-4, 1MHz | 2 | 3 |
Kerintangan Isipadu | Ω·cm 20 ℃ | 1014 | 1013 |
Kekuatan Tusukan | KV/mm , DC≥ | 20 | 20 |
Rintangan asid | mg/cm2 ≤ | 0.7 | 7 |
Tahan alkali | mg/cm2 ≤ | 0.1 | 0.2 |
Rintangan Lelasan | g/cm2 ≤ | 0.1 | 0.2 |
Kekuatan Mampatan | M Pa ≥ | 2800 | 2500 |
Kekuatan lentur | M Pa ≥ | 350 | 200 |
Modulus Elastik | G Pa | 350 | 300 |
Nisbah Poisson | 0.22 | 0.2 | |
Kekonduksian Terma | W/m·K( 20 ℃) | 25 | 20 |